X55CrMnNiN20-8 Stainless Steels to ISO 683-15 (1992)

X55CrMnNiN20-8 - Specification & Application

  • ISO 683-15 (1992) - Heat-treatable steels, alloy steels and free-cutting steels -- Part 15: Valve steels for internal combustion engines

Heat-treatable steels, alloy steels and free-cutting steels -- Part 15: Valve steels for internal combustion engines

Chemical composition(wt.%) of X55CrMnNiN20-8 grade: to ISO 683-15 (1992)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.50 0.60
Si - 0.25
Mn 7.00 10.00
P - 0.050
S - 0.030
Cr 19.50 21.50
Mo - -
Ni 1.50 2.75
N 0.20 0.40

X55CrMnNiN20-8 - Detail

Heat-treatable steels, alloy steels and free-cutting steels -- Part 15: Valve steels for internal combustion engines

Mechanical properties of grade X55CrMnNiN20-8 ISO 683-15 (1992)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
466 (≥) 593 (≥) 42 33 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 413

Physical properties of grade X55CrMnNiN20-8 ISO 683-15 (1992)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
713 (≥) 512 (≥) 42 41 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 421
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
996 272 137

Equivalent Products

We can customize the production of X55CrMnNiN20-8 grade, contact us for the best solution.