Z45CNW18-09 Stainless Steels to NF A 35-579

Z45CNW18-09 - Specification & Application

  • NF A 35-579 - Valve steels and alloys for internal combustion engines

Valve steels and alloys for internal combustion engines

Chemical composition(wt.%) of Z45CNW18-09 grade: to NF A 35-579

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.40 0.50
Si 2.00 3.00
Mn 0.80 1.50
P - 0.040
S - 0.030
Cr 17.00 19.00
Ni 8.00 10.00
Mo - -
W 0.80 1.20

Z45CNW18-09 - Detail

Valve steels and alloys for internal combustion engines

Mechanical properties of grade Z45CNW18-09 NF A 35-579

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
376 (≥) 778 (≥) 31 44 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 134

Physical properties of grade Z45CNW18-09 NF A 35-579

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
699 (≥) 995 (≥) 11 44 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 311
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
543 541 828

Equivalent Grade

Equivalent Products

We can customize the production of Z45CNW18-09 grade, contact us for the best solution.
sales@specificsteel.com