Z4CMN18-08-07Az Stainless Steels to NF A 35-578

Z4CMN18-08-07Az - Specification & Application

  • NF A 35-578 - Iron and steel. Stainless steel for high temperature application
  • NF A 36-209 - Iron and steel. Austenitic and austenic-ferritic stainless steels plates for boilers and pressure vessels

Iron and steel. Austenitic and austenic-ferritic stainless steels plates for boilers and pressure vessels

Chemical composition(wt.%) of Z4CMN18-08-07Az grade: to NF A 35-578

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.04
Si - 0.75
Mn 6.50 8.50
P - 0.040
S - 0.015
Cr 17.00 19.00
Mo - -
Ni 6.00 8.00
N 0.15 0.25

Z4CMN18-08-07Az - Detail

Iron and steel. Austenitic and austenic-ferritic stainless steels plates for boilers and pressure vessels

Mechanical properties of grade Z4CMN18-08-07Az NF A 35-578

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
626 (≥) 352 (≥) 44 42 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 332

Physical properties of grade Z4CMN18-08-07Az NF A 35-578

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
693 (≥) 588 (≥) 22 42 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 433
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
512 582 885

Equivalent Grade

Equivalent Products

We can customize the production of Z4CMN18-08-07Az grade, contact us for the best solution.