Z4CN19-10FF Stainless Steels to NF A 35-577

Z4CN19-10FF - Specification & Application

  • NF A 35-577 - Iron and steel. Stainless steel wire rods for cold forming

Iron and steel. Stainless steel wire rods for cold forming

Chemical composition(wt.%) of Z4CN19-10FF grade: to NF A 35-577

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.035
Si - 1.00
Mn - 2.00
P - 0.040
S - 0.030
Cr 18.50 20.00
Mo - -
Ni 9.00 10.00
N - 0.80
Cu - 1.00

Z4CN19-10FF - Detail

Iron and steel. Stainless steel wire rods for cold forming

Mechanical properties of grade Z4CN19-10FF NF A 35-577

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
327 (≥) 632 (≥) 13 11 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 441

Physical properties of grade Z4CN19-10FF NF A 35-577

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
463 (≥) 121 (≥) 31 21 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 332
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
136 563 698

Equivalent Products

We can customize the production of Z4CN19-10FF grade, contact us for the best solution.