Z4CND18-12-03 Stainless Steels to NF A 36-209

Z4CND18-12-03 - Specification & Application

  • NF A 36-209 - Iron and steel. Austenitic and austenic-ferritic stainless steels plates for boilers and pressure vessels

Iron and steel. Austenitic and austenic-ferritic stainless steels plates for boilers and pressure vessels

Chemical composition(wt.%) of Z4CND18-12-03 grade: to NF A 36-209

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.035
Si - 1.00
Mn - 2.00
P - 0.040
S - 0.030
Cr 17.00 18.50
Mo 2.25 2.75
Ni 11.50 12.50
N - 0.80
Cu - 1.00

Z4CND18-12-03 - Detail

Iron and steel. Austenitic and austenic-ferritic stainless steels plates for boilers and pressure vessels

Mechanical properties of grade Z4CND18-12-03 NF A 36-209

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
762 (≥) 515 (≥) 31 31 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 144

Physical properties of grade Z4CND18-12-03 NF A 36-209

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
943 (≥) 695 (≥) 23 42 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 221
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
191 987 633

Equivalent Grade

Equivalent Products

We can customize the production of Z4CND18-12-03 grade, contact us for the best solution.