Z4CNDAT13-09 Stainless Steels to NF A 35-574

Z4CNDAT13-09 - Specification & Application

  • NF A 35-574 - Iron and steel. Stainless steel for general purposes. Semi- finished products, bars and wire rod
  • NF S 94-090 - Medico-surgical equipment - Materials for ancillary positioning instruments for surgical instrument - Martensitic, precipitation hardening, austenitic and austeno-ferritic stainless steels

Medico-surgical equipment - Materials for ancillary positioning instruments for surgical instrument - Martensitic, precipitation hardening, austenitic and austeno-ferritic stainless steels

Chemical composition(wt.%) of Z4CNDAT13-09 grade: to NF A 35-574

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.040
Si - 0.10
Mn - 0.20
P - 0.015
S - 0.008
Cr 11.50 13.50
Mo 1.80 2.50
Ni 7.50 9.50
Al 0.60 1.40
Ti - 0.40

Z4CNDAT13-09 - Detail

Medico-surgical equipment - Materials for ancillary positioning instruments for surgical instrument - Martensitic, precipitation hardening, austenitic and austeno-ferritic stainless steels

Mechanical properties of grade Z4CNDAT13-09 NF A 35-574

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
397 (≥) 339 (≥) 34 34 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 331

Physical properties of grade Z4CNDAT13-09 NF A 35-574

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
798 (≥) 721 (≥) 22 22 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 233
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
251 833 644

Equivalent Grade

Equivalent Products

We can customize the production of Z4CNDAT13-09 grade, contact us for the best solution.