LW14 Stainless Steels to BS 6323-8

LW14 - Specification & Application

  • BS 6323-8 - Specification for seamless and welded steel tubes for automobile , mechanical and general engineering purposes. Specific requirements for longitudinally welded stainless steel tubes

Specification for seamless and welded steel tubes for automobile , mechanical and general engineering purposes. Specific requirements for longitudinally welded stainless steel tubes

Chemical composition(wt.%) of LW14 grade: to BS 6323-8

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si 0.20 1.00
Mn 0.50 2.00
P - 0.045
S - 0.030
Cr 17.50 19.00
Ni 9.00 12.00
Mo - -

LW14 - Detail

Specification for seamless and welded steel tubes for automobile , mechanical and general engineering purposes. Specific requirements for longitudinally welded stainless steel tubes

Mechanical properties of grade LW14 BS 6323-8

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
924 (≥) 994 (≥) 41 24 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 132

Physical properties of grade LW14 BS 6323-8

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
493 (≥) 912 (≥) 33 34 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 244
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
869 186 819

Equivalent Grade

Equivalent Products

We can customize the production of LW14 grade, contact us for the best solution.