N08366 Stainless Steels

N08366 - Specification & Application

Austenitic Ni-Cr-Mo Stainless Steel

Chemical composition(wt.%) of N08366 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.035
Mn - 2.00
Si - 1.00
P - 0.03
S - 0.03
Cr 20.00 22.00
Ni 23.50 25.50
Mo 6.00 7.00

N08366 - Detail

Austenitic Ni-Cr-Mo Stainless Steel

Mechanical properties of grade N08366

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
425 (≥) 844 (≥) 33 32 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 123

Physical properties of grade N08366

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
637 (≥) 682 (≥) 32 31 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 424
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
497 285 371

Equivalent Products

We can customize the production of N08366 grade, contact us for the best solution.
sales@specificsteel.com