NA16 Stainless Steels to BS 3072

NA16 - Specification & Application

  • BS 3072 - Specification for nickel and nickel alloys: sheet and plate
  • BS 3073 - Specification for nickel and nickel alloys: strip
  • BS 3074 - Specification for nickel and nickel alloys: seamless tube
  • BS 3076 - Specification for nickel and nickel alloys: bar

Specification for nickel and nickel alloys: bar

Chemical composition(wt.%) of NA16 grade: to BS 3072

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.05
Si - 0.50
Mn - 1.00
P - -
S - 0.030
Cr 19.50 23.50
Ni 38.00 46.00
Mo - -
Al - 0.20
Cu 1.50 3.00
Ti 0.60 1.20
Fe - -

NA16 - Detail

Specification for nickel and nickel alloys: bar

Mechanical properties of grade NA16 BS 3072

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
735 (≥) 867 (≥) 31 24 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 121

Physical properties of grade NA16 BS 3072

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
294 (≥) 987 (≥) 32 41 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 434
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
185 541 895

Equivalent Grade

Equivalent Products

We can customize the production of NA16 grade, contact us for the best solution.