NV2(1547) Stainless Steels

NV2(1547) - Specification & Application

Intake valve steel

Chemical composition(wt.%) of NV2(1547) grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.42 0.52
Si 0.15 0.30
Mn 1.25 1.75
P - 0.040
S - 0.05

NV2(1547) - Detail

Intake valve steel

Mechanical properties of grade NV2(1547)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
383 (≥) 314 (≥) 31 21 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 432

Physical properties of grade NV2(1547)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
264 (≥) 282 (≥) 34 23 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 313
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
842 925 243

Equivalent Grade

Equivalent Products