NV3/NE8150 Stainless Steels

NV3/NE8150 - Specification & Application

Intake valve steel

Chemical composition(wt.%) of NV3/NE8150 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.50
Si - 0.30
Mn - 0.80
P -
S -
Ni - 0.30
Mo - 0.15

NV3/NE8150 - Detail

Intake valve steel

Mechanical properties of grade NV3/NE8150

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
967 (≥) 787 (≥) 33 12 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 422

Physical properties of grade NV3/NE8150

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
676 (≥) 397 (≥) 31 32 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 341
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
651 363 265