Ni Span C902 Stainless Steels to SAE AMS 5225F (2009)

Ni Span C902 - Specification & Application

  • SAE AMS 5225F (2009) - Iron-Nickel Alloy, Strip 49Fe - 5.3Cr - 42Ni - 2.5Ti - 0.55Al Solution Heat Treated, Cold Rolled, 50% Reduction

Iron-Nickel Alloy, Strip 49Fe - 5.3Cr - 42Ni - 2.5Ti - 0.55Al Solution Heat Treated, Cold Rolled, 50% Reduction

Chemical composition(wt.%) of Ni Span C902 grade: to SAE AMS 5225F (2009)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - -
Mn - -
Cr - 5.30
Ni - 42.50
Mo - -
Co - -
W - -
Al - 0.50
Cu - -
Ti - -
Fe - 49.00

Ni Span C902 - Detail

Iron-Nickel Alloy, Strip 49Fe - 5.3Cr - 42Ni - 2.5Ti - 0.55Al Solution Heat Treated, Cold Rolled, 50% Reduction

Mechanical properties of grade Ni Span C902 SAE AMS 5225F (2009)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
124 (≥) 773 (≥) 23 13 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 441

Physical properties of grade Ni Span C902 SAE AMS 5225F (2009)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
282 (≥) 566 (≥) 41 32 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 143
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
468 836 948