Nichrome V Stainless Steels to SAE AMS 5682E (2006)

Nichrome V - Specification & Application

  • SAE AMS 5682E (2006) - Nickel Alloy, Corrosion and Heat-Resistant, Welding Wire 78Ni - 20Cr

Nickel Alloy, Corrosion and Heat-Resistant, Welding Wire 78Ni - 20Cr

Chemical composition(wt.%) of Nichrome V grade: to SAE AMS 5682E (2006)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si 0.75 1.60
Mn - 1.00
Cr 14.00 18.00
Ni - 57.00
Mo - -
Co - -
W - -
Al - -
Cu - -
Ti - -
Fe - remaining

Nichrome V - Detail

Nickel Alloy, Corrosion and Heat-Resistant, Welding Wire 78Ni - 20Cr

Mechanical properties of grade Nichrome V SAE AMS 5682E (2006)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
815 (≥) 288 (≥) 23 21 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 313

Physical properties of grade Nichrome V SAE AMS 5682E (2006)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
264 (≥) 913 (≥) 21 32 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 143
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
142 993 187