Nichrome V Stainless Steels to SAE AMS 5677D (1953)

Nichrome V - Specification & Application

  • SAE AMS 5677D (1953) - Alloy, Corrosion and Heat Resistant, Covered Welding Electrodes 75ni 19.5cr 1.6(Cb + Ta)

Alloy, Corrosion and Heat Resistant, Covered Welding Electrodes 75ni 19.5cr 1.6(Cb + Ta)

Chemical composition(wt.%) of Nichrome V grade: to SAE AMS 5677D (1953)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si 0.75 1.60
Mn - 2.50
Cr 19.00 21.00
Ni - remaining
Mo - -
Co - -
W - -
Al - -
Cu - -
Ti - -
Fe - 1.00
S - 0.01

Nichrome V - Detail

Alloy, Corrosion and Heat Resistant, Covered Welding Electrodes 75ni 19.5cr 1.6(Cb + Ta)

Mechanical properties of grade Nichrome V SAE AMS 5677D (1953)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
853 (≥) 244 (≥) 24 12 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 332

Physical properties of grade Nichrome V SAE AMS 5677D (1953)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
489 (≥) 433 (≥) 41 34 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 241
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
699 326 359

Equivalent Products

We can customize the production of Nichrome V grade, contact us for the best solution.