R-357.0 Stainless Steels to SFA-5.10/SFA-5.10M

R-357.0 - Specification & Application

  • SFA-5.10/SFA-5.10M - Bare aluminum and aluminum-alloy welding electrodes and rods

Bare aluminum and aluminum-alloy welding electrodes and rods

Chemical composition(wt.%) of R-357.0 grade: to SFA-5.10/SFA-5.10M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.05
Si - 0.60
Mn - 0.80
Cr - 20.00
Ni - 25.00
Mo - -
Co - -
W - -
Al - -
Cu - -
Ti - -
Fe - -
Nb - 0.60

R-357.0 - Detail

Bare aluminum and aluminum-alloy welding electrodes and rods

Mechanical properties of grade R-357.0 SFA-5.10/SFA-5.10M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
723 (≥) 293 (≥) 13 12 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 111

Physical properties of grade R-357.0 SFA-5.10/SFA-5.10M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
145 (≥) 948 (≥) 13 24 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 232
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
834 976 993

Equivalent Products

We can customize the production of R-357.0 grade, contact us for the best solution.