S.124 Stainless Steels to BS 2S 124

S.124 - Specification & Application

  • BS 2S 124 - Specification for aircraft material. 12 per cent chromium corrosion-resisting steel (free machining) (45/55 tonf/sq in: limiting ruling section 6 in)

Specification for aircraft material. 12 per cent chromium corrosion-resisting steel (free machining) (45/55 tonf/sq in: limiting ruling section 6 in)

Chemical composition(wt.%) of S.124 grade: to BS 2S 124

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.15 0.25
Si - 1.00
Mn - 1.50
P - 0.045
S 0.15 0.40
Cr 12.00 14.00
Ni - 1.00
Mo - 0.60
Nb/Ti - -
Zr - 0.60

S.124 - Detail

Specification for aircraft material. 12 per cent chromium corrosion-resisting steel (free machining) (45/55 tonf/sq in: limiting ruling section 6 in)

Mechanical properties of grade S.124 BS 2S 124

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
393 (≥) 137 (≥) 22 21 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 213

Physical properties of grade S.124 BS 2S 124

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
497 (≥) 872 (≥) 14 12 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 133
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
437 931 254

Equivalent Grade

Equivalent Products

We can customize the production of S.124 grade, contact us for the best solution.