Specification for chromium-nickel-molybdenum-vanadium heat-resisting steel billets, bars, forgings and parts (930-1130 MPa: limiting ruling section 150 mm) (Cr 12, Ni 2.5, Mo 1.7, V 0.3)
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.08 | 0.13 | ||
Si | - | 0.35 | ||
Mn | 0.50 | 0.90 | ||
P | - | 0.030 | ||
S | - | 0.025 | ||
Cr | 11.00 | 12.50 | ||
Ni | 2.00 | 3.00 | ||
Mo | 1.50 | 2.00 | ||
Nb/Ti | - | - | ||
V | 0.25 | 0.40 | ||
N | 0.020 | 0.040 |
Specification for chromium-nickel-molybdenum-vanadium heat-resisting steel billets, bars, forgings and parts (930-1130 MPa: limiting ruling section 150 mm) (Cr 12, Ni 2.5, Mo 1.7, V 0.3)
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
242 (≥) | 586 (≥) | 33 | 43 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 123 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
543 (≥) | 238 (≥) | 23 | 11 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 342 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
947 | 752 | 659 |
We can customize the production of S.151 grade, contact us for the best solution.