Specification for 12% chromium-nickel-molybdenum-vanadium heat-resisting steel bars for the manufacture of fasteners (1100-1300 MPa: limiting ruling section 50 mm)
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.08 | 0.13 | ||
Si | - | 0.35 | ||
Mn | 0.50 | 0.90 | ||
P | - | 0.030 | ||
S | - | 0.025 | ||
Cr | 11.00 | 12.50 | ||
Ni | 2.00 | 3.00 | ||
Mo | 1.50 | 2.00 | ||
Nb/Ti | - | - | ||
V | 0.25 | 0.40 | ||
N | 0.020 | 0.040 |
Specification for 12% chromium-nickel-molybdenum-vanadium heat-resisting steel bars for the manufacture of fasteners (1100-1300 MPa: limiting ruling section 50 mm)
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
432 (≥) | 142 (≥) | 21 | 23 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 323 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
178 (≥) | 675 (≥) | 43 | 11 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 231 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
824 | 216 | 259 |
We can customize the production of S.159 grade, contact us for the best solution.