Specification for chromium-nickel corrosion-resisting steel - bright bars and parts (540 MPa, limiting ruling section 160 mm) (Cr 18, Ni 10.5, controlled nitrogen content)
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.03 | ||
Si | - | 1.00 | ||
Mn | - | 2.00 | ||
P | - | 0.040 | ||
S | - | 0.030 | ||
Cr | 17.00 | 19.00 | ||
Ni | 9.00 | 12.00 | ||
Mo | - | 0.75 | ||
Nb/Ti | - | - | ||
N | - | 0.10 |
Specification for chromium-nickel corrosion-resisting steel - bright bars and parts (540 MPa, limiting ruling section 160 mm) (Cr 18, Ni 10.5, controlled nitrogen content)
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
369 (≥) | 692 (≥) | 23 | 44 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 432 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
365 (≥) | 477 (≥) | 22 | 42 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 331 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
465 | 515 | 723 |
We can customize the production of S.160 grade, contact us for the best solution.