S.536 Stainless Steels to BS S 536

S.536 - Specification & Application

  • BS S 536 - Specification for low carbon 18/10 chromium-nickel corrosion-resisting steel sheet and strip (500 MPa)

Specification for low carbon 18/10 chromium-nickel corrosion-resisting steel sheet and strip (500 MPa)

Chemical composition(wt.%) of S.536 grade: to BS S 536

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.030
Si 0.20 1.00
Mn 0.50 2.00
P - 0.035
S - 0.025
Cr 17.50 19.00
Ni 9.00 12.00
Mo - -
Nb/Ti - -

S.536 - Detail

Specification for low carbon 18/10 chromium-nickel corrosion-resisting steel sheet and strip (500 MPa)

Mechanical properties of grade S.536 BS S 536

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
877 (≥) 586 (≥) 41 34 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 424

Physical properties of grade S.536 BS S 536

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
394 (≥) 819 (≥) 23 31 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 113
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
359 533 912

Equivalent Grade

Equivalent Products

We can customize the production of S.536 grade, contact us for the best solution.