S-816 Stainless Steels to SAE J 467 (1968)

S-816 - Specification & Application

  • SAE J 467 (1968) - Special Purpose Alloys ("Superalloys")

Special Purpose Alloys ("Superalloys")

Chemical composition(wt.%) of S-816 grade: to SAE J 467 (1968)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.37
Si - 0.55
Mn - 1.50
Cr - 20.00
Ni - 20.00
Mo - 4.00
Co - remaining
W - 4.00
Al - -
Cu - -
Ti - -
Fe - 3.40
Nb - 4.00

S-816 - Detail

Special Purpose Alloys ("Superalloys")

Mechanical properties of grade S-816 SAE J 467 (1968)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
418 (≥) 946 (≥) 22 22 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 331

Physical properties of grade S-816 SAE J 467 (1968)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
484 (≥) 989 (≥) 14 44 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 213
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
838 947 176

Equivalent Grade

Equivalent Products

We can customize the production of S-816 grade, contact us for the best solution.