SA-240 N08020 Stainless Steels to SA-240/SA-240M

SA-240 N08020 - Specification & Application

  • SA-240/SA-240M - Specification for Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Specification for Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Chemical composition(wt.%) of SA-240 N08020 grade: to SA-240/SA-240M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.07
Mn - 2.00
Si - 1.00
P - 0.045
S - 0.035
Cr 19.00 21.00
Ni 32.00 38.00
Mo 2.00 3.00
Cu 3.00 4.00
Nb 8×C% 1.00

SA-240 N08020 - Detail

Specification for Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Mechanical properties of grade SA-240 N08020 SA-240/SA-240M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
822 (≥) 456 (≥) 44 32 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 141

Physical properties of grade SA-240 N08020 SA-240/SA-240M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
874 (≥) 789 (≥) 44 12 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 434
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
749 551 238

Equivalent Products

We can customize the production of SA-240 N08020 grade, contact us for the best solution.