SA-240 S31726 Stainless Steels to SA-240/SA-240M

SA-240 S31726 - Specification & Application

  • SA-240/SA-240M - Specification for Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Specification for Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Chemical composition(wt.%) of SA-240 S31726 grade: to SA-240/SA-240M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Mn - 2.00
Si - 0.75
P - 0.045
S - 0.03
Cr 17.00 20.00
Ni 13.50 17.50
Mo 4.00 5.00
N 0.10 0.20

SA-240 S31726 - Detail

Specification for Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Mechanical properties of grade SA-240 S31726 SA-240/SA-240M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
763 (≥) 332 (≥) 41 13 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 323

Physical properties of grade SA-240 S31726 SA-240/SA-240M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
843 (≥) 828 (≥) 41 24 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 443
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
256 457 198

Equivalent Products

We can customize the production of SA-240 S31726 grade, contact us for the best solution.
sales@specificsteel.com