SA-249 S34565 Stainless Steels to SA-249/SA-249M

SA-249 S34565 - Specification & Application

  • SA-249/SA-249M - Specification for Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes

Specification for Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes

Chemical composition(wt.%) of SA-249 S34565 grade: to SA-249/SA-249M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Mn 5.00 7.00
Si - 1.00
P - 0.03
S - 0.01
Cr 23.00 25.00
Ni 16.00 18.00
Mo 4.00 5.00
N 0.40 0.60
Nb - 0.10

SA-249 S34565 - Detail

Specification for Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes

Mechanical properties of grade SA-249 S34565 SA-249/SA-249M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
412 (≥) 752 (≥) 11 11 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 143

Physical properties of grade SA-249 S34565 SA-249/SA-249M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
575 (≥) 646 (≥) 11 12 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 234
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
424 957 372

Equivalent Products

We can customize the production of SA-249 S34565 grade, contact us for the best solution.