SA-249 TP310H Stainless Steels to SA-249/SA-249M

SA-249 TP310H - Specification & Application

  • SA-249/SA-249M - Specification for Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes

Specification for Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes

Chemical composition(wt.%) of SA-249 TP310H grade: to SA-249/SA-249M

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.10
Si - 0.75
Mn - 2.00
P - 0.045
S - 0.03
Cr 24.00 26.00
Ni 19.00 22.00

SA-249 TP310H - Detail

Specification for Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes

Mechanical properties of grade SA-249 TP310H SA-249/SA-249M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
291 (≥) 312 (≥) 33 33 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 424

Physical properties of grade SA-249 TP310H SA-249/SA-249M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
952 (≥) 342 (≥) 24 41 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 224
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
733 531 892

Equivalent Products

We can customize the production of SA-249 TP310H grade, contact us for the best solution.