SA-358 N08020 Stainless Steels to SA-358/SA-358M

SA-358 N08020 - Specification & Application

  • SA-358/SA-358M - Electric-Fusion-Welded Austenitic Chromium-Nickel Alloy Steel Pipe for High-Temperature Service

Electric-Fusion-Welded Austenitic Chromium-Nickel Alloy Steel Pipe for High-Temperature Service

Chemical composition(wt.%) of SA-358 N08020 grade: to SA-358/SA-358M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.07
Mn - 2.00
Si - 1.00
P - 0.045
S - 0.035
Cr 19.00 21.00
Ni 32.00 38.00
Mo 2.00 3.00
Cu 3.00 4.00
Nb 8×C% 1.00

SA-358 N08020 - Detail

Electric-Fusion-Welded Austenitic Chromium-Nickel Alloy Steel Pipe for High-Temperature Service

Mechanical properties of grade SA-358 N08020 SA-358/SA-358M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
228 (≥) 424 (≥) 33 43 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 331

Physical properties of grade SA-358 N08020 SA-358/SA-358M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
893 (≥) 667 (≥) 13 13 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 244
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
469 525 719

Equivalent Products