SA-403 S20910 Stainless Steels to SA-403/SA-403M

SA-403 S20910 - Specification & Application

  • SA-403/SA-403M - Specification for Wrought Austenitic Stainless Steel Piping Fittings

Specification for Wrought Austenitic Stainless Steel Piping Fittings

Chemical composition(wt.%) of SA-403 S20910 grade: to SA-403/SA-403M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.06
Mn 4.00 6.00
Si - 1.00
P - 0.04
S - 0.03
Cr 20.50 23.50
Ni 11.50 13.50
Mo 1.50 3.00
N 0.20 0.40
Nb 0.10 0.30
V 0.10 0.30

SA-403 S20910 - Detail

Specification for Wrought Austenitic Stainless Steel Piping Fittings

Mechanical properties of grade SA-403 S20910 SA-403/SA-403M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
945 (≥) 925 (≥) 44 32 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 113

Physical properties of grade SA-403 S20910 SA-403/SA-403M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
899 (≥) 988 (≥) 41 12 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 414
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
746 531 124