SA-409 N08367 Stainless Steels to SA-409/SA-409M

SA-409 N08367 - Specification & Application

  • SA-409/SA-409M - Welded Large Diameter Austenitic Steel Pipe for Corrosive or High-Temperature Service

Welded Large Diameter Austenitic Steel Pipe for Corrosive or High-Temperature Service

Chemical composition(wt.%) of SA-409 N08367 grade: to SA-409/SA-409M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Mn - 2.00
Si - 1.00
P - 0.04
S - 0.03
Cr 20.00 22.00
Ni 23.50 25.50
Mo 6.00 7.00
N 0.18 0.25

SA-409 N08367 - Detail

Welded Large Diameter Austenitic Steel Pipe for Corrosive or High-Temperature Service

Mechanical properties of grade SA-409 N08367 SA-409/SA-409M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
524 (≥) 217 (≥) 22 12 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 423

Physical properties of grade SA-409 N08367 SA-409/SA-409M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
569 (≥) 936 (≥) 33 42 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 234
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
595 837 165
We can customize the production of SA-409 N08367 grade, contact us for the best solution.