SA-790 S31500 Stainless Steels to SA-790/SA-790M

SA-790 S31500 - Specification & Application

  • SA-790/SA-790M - Specification for Seamless and Welded Ferritic /Austenitic Stainless Steel Pipe

Specification for Seamless and Welded Ferritic /Austenitic Stainless Steel Pipe

Chemical composition(wt.%) of SA-790 S31500 grade: to SA-790/SA-790M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Mn 1.20 2.00
Si 1.40 2.00
P - 0.03
S - 0.03
Cr 18.00 19.00
Ni 4.25 5.25
Mo 2.50 3.00

SA-790 S31500 - Detail

Specification for Seamless and Welded Ferritic /Austenitic Stainless Steel Pipe

Mechanical properties of grade SA-790 S31500 SA-790/SA-790M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
945 (≥) 131 (≥) 34 23 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 431

Physical properties of grade SA-790 S31500 SA-790/SA-790M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
826 (≥) 347 (≥) 12 44 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 123
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
399 461 343

Equivalent Products

We can customize the production of SA-790 S31500 grade, contact us for the best solution.
sales@specificsteel.com