SA-790 S32520 Stainless Steels to SA-790/SA-790M

SA-790 S32520 - Specification & Application

  • SA-790/SA-790M - Specification for Seamless and Welded Ferritic /Austenitic Stainless Steel Pipe

Specification for Seamless and Welded Ferritic /Austenitic Stainless Steel Pipe

Chemical composition(wt.%) of SA-790 S32520 grade: to SA-790/SA-790M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Mn - 1.50
Si - 0.80
P - 0.035
S - 0.02
Cr 24.00 26.00
Ni 5.50 8.00
Mo 3.00 5.00
N 0.20 0.35
Cu 0.05 3.00

SA-790 S32520 - Detail

Specification for Seamless and Welded Ferritic /Austenitic Stainless Steel Pipe

Mechanical properties of grade SA-790 S32520 SA-790/SA-790M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
336 (≥) 576 (≥) 11 31 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 224

Physical properties of grade SA-790 S32520 SA-790/SA-790M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
351 (≥) 557 (≥) 31 33 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 444
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
526 762 474

Equivalent Products

We can customize the production of SA-790 S32520 grade, contact us for the best solution.
sales@specificsteel.com