SA-790 S32950 Stainless Steels to SA-790/SA-790M

SA-790 S32950 - Specification & Application

  • SA-790/SA-790M - Specification for Seamless and Welded Ferritic /Austenitic Stainless Steel Pipe

Specification for Seamless and Welded Ferritic /Austenitic Stainless Steel Pipe

Chemical composition(wt.%) of SA-790 S32950 grade: to SA-790/SA-790M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Mn - 2.00
Si - 0.60
P - 0.035
S - 0.01
Cr 26.00 29.00
Ni 3.50 5.20
Mo 1.00 2.50
N 0.15 0.25

SA-790 S32950 - Detail

Specification for Seamless and Welded Ferritic /Austenitic Stainless Steel Pipe

Mechanical properties of grade SA-790 S32950 SA-790/SA-790M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
832 (≥) 183 (≥) 21 43 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 241

Physical properties of grade SA-790 S32950 SA-790/SA-790M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
813 (≥) 865 (≥) 23 23 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 122
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
331 815 698