SA-814 S31254 Stainless Steels to SA-814/SA-814M

SA-814 S31254 - Specification & Application

  • SA-814/SA-814M - Specification for Cold-Worked Welded Austenitic Stainless Steel Pipe

Specification for Cold-Worked Welded Austenitic Stainless Steel Pipe

Chemical composition(wt.%) of SA-814 S31254 grade: to SA-814/SA-814M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.02
Mn - 1.00
Si - 0.80
P - 0.03
S - 0.01
Cr 19.50 20.50
Ni 17.50 18.50
Mo 6.00 6.50
Cu 0.50 1.00
N 0.18 0.22

SA-814 S31254 - Detail

Specification for Cold-Worked Welded Austenitic Stainless Steel Pipe

Mechanical properties of grade SA-814 S31254 SA-814/SA-814M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
125 (≥) 922 (≥) 42 42 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 123

Physical properties of grade SA-814 S31254 SA-814/SA-814M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
134 (≥) 141 (≥) 42 43 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 321
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
593 347 967

Equivalent Products

We can customize the production of SA-814 S31254 grade, contact us for the best solution.