SA-815 WPS32760 Stainless Steels to SA-815/SA-815M

SA-815 WPS32760 - Specification & Application

  • SA-815/SA-815M - Specification for Wrought Ferritic, Ferritic /Austenitic, and Martensitic Stainless Steel Piping Fittings

Specification for Wrought Ferritic, Ferritic /Austenitic, and Martensitic Stainless Steel Piping Fittings

Chemical composition(wt.%) of SA-815 WPS32760 grade: to SA-815/SA-815M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Mn - 1.00
Si - 1.00
P - 0.03
S - 0.01
Cr 24.00 26.00
Ni 6.00 8.00
Mo 3.00 4.00

SA-815 WPS32760 - Detail

Specification for Wrought Ferritic, Ferritic /Austenitic, and Martensitic Stainless Steel Piping Fittings

Mechanical properties of grade SA-815 WPS32760 SA-815/SA-815M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
732 (≥) 637 (≥) 24 42 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 133

Physical properties of grade SA-815 WPS32760 SA-815/SA-815M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
389 (≥) 248 (≥) 43 44 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 441
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
143 851 525