SA-965 S32109 Stainless Steels to SA-965/SA-965M

SA-965 S32109 - Specification & Application

  • SA-965/SA-965M - Specification for Steel Forgings, Austenitic, for Pressure and High Temperature Parts

Specification for Steel Forgings, Austenitic, for Pressure and High Temperature Parts

Chemical composition(wt.%) of SA-965 S32109 grade: to SA-965/SA-965M

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.10
Mn - 2.00
Si - 1.00
P - 0.04
S - 0.03
Cr 17.00 20.00
Ni 9.00 12.00

SA-965 S32109 - Detail

Specification for Steel Forgings, Austenitic, for Pressure and High Temperature Parts

Mechanical properties of grade SA-965 S32109 SA-965/SA-965M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
176 (≥) 159 (≥) 11 22 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 422

Physical properties of grade SA-965 S32109 SA-965/SA-965M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
724 (≥) 468 (≥) 31 13 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 323
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
521 537 434

Equivalent Products

We can customize the production of SA-965 S32109 grade, contact us for the best solution.
sales@specificsteel.com