SB-464 N08020 Stainless Steels to SB-464

SB-464 N08020 - Specification & Application

  • SB-464 - Standard Specification for Welded UNS N08020 Alloy Pipe

Standard Specification for Welded UNS N08020 Alloy Pipe

Chemical composition(wt.%) of SB-464 N08020 grade: to SB-464

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.07
Mn - 2.00
Si - 1.00
P - 0.045
S - 0.035
Cr 19.00 21.00
Ni 32.00 38.00
Mo 2.00 3.00
Cu 3.00 4.00
Nb 8×C% 1.00

SB-464 N08020 - Detail

Standard Specification for Welded UNS N08020 Alloy Pipe

Mechanical properties of grade SB-464 N08020 SB-464

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
176 (≥) 529 (≥) 33 34 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 234

Physical properties of grade SB-464 N08020 SB-464

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
982 (≥) 243 (≥) 13 12 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 421
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
521 467 786

Equivalent Products

We can customize the production of SB-464 N08020 grade, contact us for the best solution.