SB-619 R20033 Stainless Steels to SB-619

SB-619 R20033 - Specification & Application

  • SB-619 - Standard Specification for Welded Nickel and Nickel-Cobalt Alloy Pipe

Standard Specification for Welded Nickel and Nickel-Cobalt Alloy Pipe

Chemical composition(wt.%) of SB-619 R20033 grade: to SB-619

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.12
Si - 0.30
Mn - 0.80
Cr - 19.00
Ni - 14.00
Mo - -
Co - -
W - -
Al - -
Cu - -
Ti - -
Fe - remaining
Nb - 1.60

SB-619 R20033 - Detail

Standard Specification for Welded Nickel and Nickel-Cobalt Alloy Pipe

Mechanical properties of grade SB-619 R20033 SB-619

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
156 (≥) 733 (≥) 43 22 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 243

Physical properties of grade SB-619 R20033 SB-619

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
237 (≥) 198 (≥) 22 41 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 111
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
937 581 481

Equivalent Products

We can customize the production of SB-619 R20033 grade, contact us for the best solution.