STS316FB Stainless Steels to D 3691 (2001)

STS316FB - Specification & Application

  • D 3691 (2001) - Stainless steel blooms and billets for forgings

Stainless steel blooms and billets for forgings

Chemical composition(wt.%) of STS316FB grade: to D 3691 (2001)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.030
Cr 16.00 18.00
Ni 10.00 14.00
Mo 2.00 3.00
N - -

STS316FB - Detail

Stainless steel blooms and billets for forgings

Mechanical properties of grade STS316FB D 3691 (2001)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
251 (≥) 134 (≥) 44 42 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 323

Physical properties of grade STS316FB D 3691 (2001)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
232 (≥) 659 (≥) 33 34 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 333
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
779 841 773

Equivalent Products

We can customize the production of STS316FB grade, contact us for the best solution.