SUS 329J 3L Stainless Steels to G 4303 (2012)

SUS 329J 3L - Specification & Application

  • G 4303 (2012) - Stainless steel bars

Stainless steel bars

Chemical composition(wt.%) of SUS 329J 3L grade: to G 4303 (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 1.00
Mn - 2.00
P - 0.04
S - 0.03
Cr 21.00 24.00
Ni 4.50 6.50
Mo 2.50 3.50
N 0.08 0.20

SUS 329J 3L - Detail

Stainless steel bars

Mechanical properties of grade SUS 329J 3L G 4303 (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
758 (≥) 297 (≥) 13 32 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 242

Physical properties of grade SUS 329J 3L G 4303 (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
734 (≥) 779 (≥) 12 22 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 122
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
544 397 638

Equivalent Products

We can customize the production of SUS 329J 3L grade, contact us for the best solution.
sales@specificsteel.com