SUS 410 Stainless Steels to G 4305 (2012)

SUS 410 - Specification & Application

  • G 4305 (2012) - Cold-rolled stainless steel plate, sheet and strip

Cold-rolled stainless steel plate, sheet and strip

Chemical composition(wt.%) of SUS 410 grade: to G 4305 (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 1.00
Mn - 1.00
P - 0.04
S - 0.03
Cr 11.50 13.50
Ni - 0.60
Mo - -
N - -

SUS 410 - Detail

Cold-rolled stainless steel plate, sheet and strip

Mechanical properties of grade SUS 410 G 4305 (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
123 (≥) 317 (≥) 12 22 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 413

Physical properties of grade SUS 410 G 4305 (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
567 (≥) 592 (≥) 33 43 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 132
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
132 264 653