SUS 430 F Stainless Steels to G 4309 (1999)

SUS 430 F - Specification & Application

  • G 4309 (1999) - Stainless steel wires

Stainless steel wires

Chemical composition(wt.%) of SUS 430 F grade: to G 4309 (1999)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.12
Si - 1.00
Mn - 1.25
P - 0.06
S - 0.15
Cr 16.00 18.00
Ni - 0.60

SUS 430 F - Detail

Stainless steel wires

Mechanical properties of grade SUS 430 F G 4309 (1999)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
352 (≥) 532 (≥) 42 41 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 134

Physical properties of grade SUS 430 F G 4309 (1999)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
472 (≥) 633 (≥) 44 44 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 111
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
278 123 273

Equivalent Products

We can customize the production of SUS 430 F grade, contact us for the best solution.