Stainless W Stainless Steels to SAE J 467 (1968)

Stainless W - Specification & Application

  • SAE J 467 (1968) - Special Purpose Alloys ("Superalloys")

Special Purpose Alloys ("Superalloys")

Chemical composition(wt.%) of Stainless W grade: to SAE J 467 (1968)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.06
Si - 0.60
Mn - 0.55
Cr - 17.00
Ni - 7.00
Mo - -
Co - -
W - -
Al - 0.20
Cu - -
Ti - 0.80
Fe - remaining
N - 0.02

Stainless W - Detail

Special Purpose Alloys ("Superalloys")

Mechanical properties of grade Stainless W SAE J 467 (1968)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
457 (≥) 312 (≥) 22 24 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 411

Physical properties of grade Stainless W SAE J 467 (1968)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
322 (≥) 238 (≥) 23 23 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 244
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
841 623 331

Equivalent Grade

Equivalent Products

We can customize the production of Stainless W grade, contact us for the best solution.
sales@specificsteel.com