Stellite X90 Tool Die Steels

Stellite X90 - Specification & Application

Stellite alloy

Chemical composition(wt.%) of Stellite X90 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.50
Si - -
Mn - -
Cr - 26.00
Ni - 10.00
Mo - -
Co remaining -
W - 7.00
Fe - -

Stellite X90 - Detail

Stellite alloy

Mechanical properties of grade Stellite X90

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
521 (≥) 398 (≥) 14 23 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 132

Physical properties of grade Stellite X90

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
872 (≥) 992 (≥) 14 42 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 434
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
858 586 234

Equivalent Grade

Equivalent Products

We can customize the production of Stellite X90 grade, contact us for the best solution.
sales@specificsteel.com