UNITEMP 750 Stainless Steels to SAE J 470 (1976)

UNITEMP 750 - Specification & Application

  • SAE J 470 (1976) - Wrought nickel and nickel-related alloys

Wrought nickel and nickel-related alloys

Chemical composition(wt.%) of UNITEMP 750 grade: to SAE J 470 (1976)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.04
Si - -
Mn - -
Cr - 15.50
Ni - remaining
Mo - -
Co - -
W - -
Al - 1.20
Cu - -
Ti - 2.30
Fe - 7.00
Nb - 1.00
B - 0.003

UNITEMP 750 - Detail

Wrought nickel and nickel-related alloys

Mechanical properties of grade UNITEMP 750 SAE J 470 (1976)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
435 (≥) 842 (≥) 32 31 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 313

Physical properties of grade UNITEMP 750 SAE J 470 (1976)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
646 (≥) 675 (≥) 22 34 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 124
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
496 758 947

Equivalent Grade

Equivalent Products

We can customize the production of UNITEMP 750 grade, contact us for the best solution.
sales@specificsteel.com