V-36 Stainless Steels to SAE J 467 (1968)

V-36 - Specification & Application

  • SAE J 467 (1968) - Special Purpose Alloys ("Superalloys")

Special Purpose Alloys ("Superalloys")

Chemical composition(wt.%) of V-36 grade: to SAE J 467 (1968)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.29
Si - 0.50
Mn - 0.60
Cr - 25.00
Ni - 20.00
Mo - 4.00
Co - remaining
W - 2.00
Al - -
Cu - -
Ti - -
Fe - 2.40
Nb - 2.00

V-36 - Detail

Special Purpose Alloys ("Superalloys")

Mechanical properties of grade V-36 SAE J 467 (1968)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
524 (≥) 758 (≥) 23 13 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 214

Physical properties of grade V-36 SAE J 467 (1968)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
295 (≥) 937 (≥) 32 33 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 322
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
518 265 957

Equivalent Grade

Equivalent Products

We can customize the production of V-36 grade, contact us for the best solution.