V-57 Stainless Steels to SAE J 467 (1968)

V-57 - Specification & Application

  • SAE J 467 (1968) - Special Purpose Alloys ("Superalloys")

Special Purpose Alloys ("Superalloys")

Chemical composition(wt.%) of V-57 grade: to SAE J 467 (1968)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.05
Si - 0.35
Mn - 0.20
Cr - 14.75
Ni - 27.25
Mo - 1.30
Co - -
W - -
Al - 0.20
Cu - -
Ti - 3.00
Fe - remaining
V - 0.30
B - 0.01

V-57 - Detail

Special Purpose Alloys ("Superalloys")

Mechanical properties of grade V-57 SAE J 467 (1968)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
863 (≥) 331 (≥) 33 34 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 424

Physical properties of grade V-57 SAE J 467 (1968)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
612 (≥) 817 (≥) 33 42 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 224
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
896 723 273