Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode Remelted or Vacuum Induction Melted 1825 to 1900°F (996 to 1038°C) Solution, Stabilization, and Pre
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.07 | ||
Si | - | 0.10 | ||
Mn | - | 0.10 | ||
Cr | - | 19.75 | ||
Ni | - | remaining | ||
Mo | - | 4.45 | ||
Co | - | 14.00 | ||
W | - | - | ||
Al | - | 1.40 | ||
Cu | - | - | ||
Ti | - | 3.00 | ||
Fe | - | 0.75 | ||
B | - | 0.005 | ||
Zr | - | 0.04 |
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode Remelted or Vacuum Induction Melted 1825 to 1900°F (996 to 1038°C) Solution, Stabilization, and Precipitation Heat Treated
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
122 (≥) | 493 (≥) | 14 | 41 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 133 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
544 (≥) | 952 (≥) | 34 | 11 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 342 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
358 | 212 | 264 |
We can customize the production of Waspaloy grade, contact us for the best solution.