X6NiCrSiNCe35-25 Stainless Steels to BS EN 10088-1

X6NiCrSiNCe35-25 - Specification & Application

  • BS EN 10088-1 - Stainless steels - Part 1: List of stainless steels
  • BS EN 10095 - Heat resisting steels and nickel alloys
  • BS EN 10296-2 (2005) - Welded circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 2: Stainless steel
  • BS EN 10297-2 (2005) - Seamless circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 2: Stainless steel

Seamless circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 2: Stainless steel

Chemical composition(wt.%) of X6NiCrSiNCe35-25 grade: to BS EN 10088-1

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.08
Si 1.20 2.00
Mn - 2.00
P - 0.040
S - 0.015
Cr 24.00 26.00
Ni 34.00 36.00
Al - -
Ce 0.03 0.08
N 0.12 0.20

X6NiCrSiNCe35-25 - Detail

Seamless circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 2: Stainless steel

Mechanical properties of grade X6NiCrSiNCe35-25 BS EN 10088-1

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
682 (≥) 945 (≥) 13 12 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 344

Physical properties of grade X6NiCrSiNCe35-25 BS EN 10088-1

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
428 (≥) 468 (≥) 14 43 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 314
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
447 146 972

Equivalent Grade

Equivalent Products