Steel tubes. Seamless austenitic steel tubes for use at high temperatures. Dimensions (with normal tolerances). Technical conditions of delivery
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.07 | 0.12 | ||
Si | - | 0.75 | ||
Mn | - | 1.00 | ||
P | - | 0.040 | ||
S | - | 0.015 | ||
Cr | 16.00 | 18.00 | ||
Mo | 12.00 | 14.00 | ||
Ni | - | - | ||
B | 0.0015 | 0.0060 | ||
W | 2.50 | 4.00 | ||
Ti | 4(C+N) | 0.70 |
Steel tubes. Seamless austenitic steel tubes for use at high temperatures. Dimensions (with normal tolerances). Technical conditions of delivery
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
932 (≥) | 591 (≥) | 21 | 31 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 431 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
556 (≥) | 649 (≥) | 32 | 32 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 132 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
981 | 853 | 132 |
We can customize the production of Z10CNWT17-13B grade, contact us for the best solution.