Z1CN25-20 Stainless Steels to NF A 35-573

Z1CN25-20 - Specification & Application

  • NF A 35-573 - Stainless steels for general purposes. Plates, wide strips and strips
  • NF A 36-209 - Iron and steel. Austenitic and austenic-ferritic stainless steels plates for boilers and pressure vessels
  • NF A 49-244 - Steel tubes - Welded austenitic stainless and austenitic ferritic steel rolled tubes for pressure service - Dimensions, technical conditions for delivery

Steel tubes - Welded austenitic stainless and austenitic ferritic steel rolled tubes for pressure service - Dimensions, technical conditions for delivery

Chemical composition(wt.%) of Z1CN25-20 grade: to NF A 35-573

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.015
Si - 0.40
Mn - 2.00
P - 0.025
S - 0.010
Cr 24.00 26.00
Mo - 0.50
Ni 19.00 22.00

Z1CN25-20 - Detail

Steel tubes - Welded austenitic stainless and austenitic ferritic steel rolled tubes for pressure service - Dimensions, technical conditions for delivery

Mechanical properties of grade Z1CN25-20 NF A 35-573

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
732 (≥) 479 (≥) 22 31 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 321

Physical properties of grade Z1CN25-20 NF A 35-573

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
571 (≥) 662 (≥) 13 32 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 431
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
892 398 879

Equivalent Products

We can customize the production of Z1CN25-20 grade, contact us for the best solution.