04X18H10 Stainless Steels

04X18H10 - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 04X18H10 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.04
Si - 0.80
Mn - 2.00
P - 0.035
S - 0.020
Cr 17.00 19.00
Ni 9.00 11.00
Mo - 0.30
W - 0.20
Ti - 0.20

04X18H10 - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 04X18H10

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
128 (≥) 856 (≥) 33 12 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 423

Physical properties of grade 04X18H10

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
937 (≥) 614 (≥) 23 22 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 213
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
538 288 997

Equivalent Grade

Equivalent Products

We can customize the production of 04X18H10 grade, contact us for the best solution.